+99450 312 24 56 Baku city. Narimanov r/nu, Ziya Bunyadov Ave. 108 C. lismankazimov@kleber.az
Az Ru

Glue 300.0

Industrial adhesive for waterproof
connections in accordance with DIN EN 204,
gluing quality D3
Application area
• Bonding of windows and doors
• Bonding of HPL boards across the surface
• Bonding of separating materials along the surface
walls and production of elements
• Bonding of hard and exotic rocks
wood, for example in construction
stairs
• Suitable for gluing veneer
• High frequency bonding

Advantages
• As a one-component adhesive – supplied
in finished form
• Suitable for warm and cold
gluing
• Short pressing time
Properties of the adhesive connection
• KLEIBERIT 300.0 as one-component
adhesive according to DIN EN 204 corresponds to the group
load D3
• High adhesive strength also with
gluing hard and exotic rocks
wood
• Adhesive seam: viscous-hard, colorless
Glue properties
Base: PVA dispersion
Density: about 1.10 g/cm3
pH value: 3 ± 0.5
Glue color: white
Consistency: medium viscous
Viscosity at 20°C
-Brookfield RVT Sp.6/20 rpm:
12.000 ± 3.000 mPa.s
Open time
at 20°C: 6-10 minutes
Whitening point: approx. + 5°C
Marking: not subject to marking
according to EU regulations
(see safety data sheet)

Application methods
• Brush, spatula or glue application
roller
• Glue-applying devices in frames
presses and splicing installations
mini spike
• Gluing installations
Gluing devices must be
made of stainless steel or
synthetic materials.
Recycling
The materials to be glued must be
dust free, degreased and
acclimatized. Optimal temperature
processing 18-20 °C, optimal humidity
wood – 8 – 10% for use
indoors, 10 – 14% during production
windows Do not process at temperatures
below +10 °C. Usually enough
one-sided application of glue. At
gluing hard and exotic wood
breeds, double-sided application is recommended
glue.
Application quantity:
100 - 130 g/m2 when gluing veneer
150 - 200 g/m2 when gluing massive
wood
Glue consumption depends on the surface structure
and on the application devices used
glue.
Open time: 6 - 10 minutes
Open time depends on
amount of application, absorbency
material, wood and air humidity, and
also room temperature.
Press pressure: 0.7 - 1N/mm2 at
gluing lamellas or laminated wood
Pressing time:
Application Temperature Time
pressing
Bonding fugues 20 °C from 15 min.
Fugue bonding
(preliminary
heating):

50 °C from 5 min.

Bonding fugues 80 °C from 2 min.
Gluing by
HPL plates

20 °C 15-20 min.

Gluing by
HPL plates

50 °C approx. 5 min.

Gluing by
HPL plates

80 °C 1-2 min.

According to DIN/EN 204 final
strength according to load groups
achieved after 7 days.
Wood and wood materials are
natural substances. Based
various compositions contained in wood
substances (depending on location
growth, pre-treatment) in
in some cases (for example, beech, cherry,
maple) the color of the wood may change.
In addition, when gluing wood,
containing tannins (for example,
oak) and in case of contact with iron (for example,
when using the wrong one
pressing devices) can also
color change occurs.
Cleaning
Cleaning of glue application equipment
devices and containers for glue
materials is carried out with water.
Package
KLEIBERIT 300.0:
Plastic bucket 10 kg net
Plastic bucket 28 kg net
Plastic drum 130 kg net
Plastic container (disposable)
1000 kg net
Storage
KLEIBERIT 300.0 is stored at 20°C in
The original unopened packaging is about 1 year old.
One-time exposure to low temperatures is acceptable
temperatures during transportation up to -30 °C.
Before processing, carefully bring the glue
up to room temperature and good
mix.